Suhm Spring Works - Materials Properties
Material |
Material
Properties |
Maximum
Working Temp. |
|
Modulus
of Elasticity |
Approx.
Design % of Ultimate Tensile (torsional) |
Common
Sizes, |
Inconel 718 Bar ASTM B637 UNS N07718 |
Age
hardened. Good corrosion
resistance. Good for use in elevated
temperature applications. No magnetism |
1200°F |
250/210 |
(E) 29 (G) 11.2 |
45% |
.234"
to 1.500" |
Bar Diameter, in |
|||
.234 | .406 | .687 | .885 |
.250 | .562 | .734 | 1.420 |
.281 | .573 | .750 | 1.500 |
.359 | .625 | .875 |
COMMENTS: |
There
is currently not a standard/specification
which covers tensile/yield strength values for
spring tempered wire. Tensile
strength should be comparable to Inconel X750, however
please check with a Suhm representative
for actual strength values. |
These data are provided as a reference guide only and are not intended for design purposes. Strength values and sizes are subject to change. Please check with a Suhm Spring representative for confirmation.