Suhm Spring Works - Materials Properties
Material |
Material
Properties |
Maximum
Working Temp. |
|
Modulus
of Elasticity |
Approx.
Design % of Ultimate Tensile (torsional) |
Common
Sizes |
Inconel 718 Bar ASTM B637 UNS N07718 |
Age
hardened. Good corrosion
resistance. Good for use in elevated
temperature applications. No magnetism |
649°C |
1724/1448 |
(E) 200k (G) 77,2k |
45% |
5,94
to 38,10 |
Bar Diameter, mm |
|||
5,94 | 10,31 | 17,45 | 22,48 |
6,35 | 14,27 | 18,64 | 36,07 |
7,14 | 14,55 | 19,05 | 38,10 |
9,12 | 15,88 | 22,23 |
COMMENTS: |
There
is currently not a standard/specification
which covers tensile/yield strength values for
spring tempered wire. Tensile
strength should be comparable to Inconel X750, however
please check with a Suhm representative
for actual strength values. Larger sizes can be
attained in the spring tempered conditions. Also
bar stock is available in the solution annealed/aged condition. Check
with a Suhm representative for further
information. |
These data are provided as a reference guide only and are not intended for design purposes. Strength values and sizes are subject to change. Please check with a Suhm Spring representative for confirmation.